等离子体

LSPR Nanosensors with Highly Ordered Gold Nanoparticles Fabricated on Nanodimpled Aluminium Templates

ty10086 提交于 周四, 08/26/2021 - 13:26
Abstract(#br)The fabrication and characterization of a localized surface plasmon resonance (LSPR) based optical nanosensor, which utilizes highly ordered gold nanoparticles as transducers are presented in this work. The nanoparticles are synthetized using nanodimpled aluminium templates, which were prepared by a selective chemical etching of the porous anodic alumina grown over an aluminium sheet. The formed nanoparticles were directly transferred to PDMS (polydimethylsiloxane) based microfluidic cells, where their LSPR transmittance spectra were measured.

等离子体预处理对PDMS基体上DLC涂层摩擦学性能的影响。

ty10086 提交于 周三, 08/25/2021 - 16:09
利用等离子体技术在PDMS (聚二甲基硅氧烷)基片上沉积碳涂层的过程被广泛应用于从电子到生物的大量研究中。因此,对其功能性质,包括摩擦学性能的潜在改善显得非常有趣。本文分析了等离子体预处理对制备的类金刚石( DLC )涂层性能的影响,包括摩擦系数和磨损率系数的变化。采用基于低压等离子体( RF PACVD、射频等离子体辅助化学气相沉积)和介质阻挡放电( DBD )等离子体两种不同技术进行初始改性处理。测定了上述处理对PDMS表面几何结构及其水接触角和稳定性随时间变化的影响。将未改性基底上制备的DLC涂层的基本性能与等离子体预处理后的涂层进行对比。在摩擦学性能方面,DBD工艺和DLC涂层的制备后取得了最有趣的效果,磨损率降低到2.45×10 - 8 mm3 / Nm。

基于二元亲水疏水PDMS修饰的纳米通道电极对复杂基质中咖啡因的无干扰检测。

ty10086 提交于 周三, 08/25/2021 - 15:53
本研究采用等离子体引发聚二甲基硅氧烷( PDMS )沉积在二氧化硅纳米通道负载的氧化铟锡电极上,制备了一种新型的直接检测粗样品中咖啡因的电化学传感器。沉积的PDMS既含有原始的疏水的PDMS低聚物,也含有氧化的亲水性PDMS低聚物。用这两种润湿性相反的PDMS修饰的纳米通道只允许咖啡因等小两亲性分子通过,而其他亲水、疏水、大分子均被排斥。该修饰纳米通道电极具有良好的屏蔽性能,具有良好的抗干扰能力和防污染能力,可直接用于茶叶、牛奶、咖啡、焦炭等实际粗制品中咖啡因的检测,无需样品前处理。此外,该修饰电极具有良好的重复性和稳定性。相比之下,这些未经处理的样品直接使用常规电极时,观察到严重的干扰。咖啡因的线性范围在50 ~ 700μmol / L之间,检出限为20 nmol / L,该传感器为特定两亲性化合物的无干扰、无污垢分析提供了一种非常简单、快速、经济有效的方法,可扩展到广泛的应用。