Syntheses of siloxane-grafted aromatic polymers and the application to pervaporation membrane

由 ty10086 提交于 周四, 08/26/2021 - 12:56
Abstract\n\t\t\t\t\n\t\t\t\t\tThe syntheses of siloxane-grafted poly(amide-imide) and polyamide were carried out by a macromonomer method, in order to develop a highly permeable and durable membrane material for pervaporation. A novel compound, 3,5-bis(4-aminophenoxy)benzyloxypropyl-terminated polydimethylsiloxane (\n\t\t\t\t\t\tBAPB-\n\t\t\t\t\t\tPDMS), was synthesized as a macromonomer.

Synthesis and properties of polystyrene/polydimethylsiloxane graft copolymers

由 ty10086 提交于 周四, 08/26/2021 - 12:55
Polystyrene-graft-polydimethylsiloxane (PS-g-PDMS) copolymers with different PDMS content were syn-thesized by the radical bulk copolymerization of PDMS macromonomer and styrene. The copolymers were charac-terized by Fourier transform infrared (FT-IR),1H-nuclear magnetic resonance (NMR), thermogravimetric analysis (TGA), dynamic mechanical analysis (DMA), transmission electron microscopy (TEM) and the mechanical properties of the copolymers were also carried out.

混合接枝嵌段共聚物结构启用的高效室温固态锂离子导体

由 ty10086 提交于 周三, 08/25/2021 - 17:03
在广泛的室温场景下,固态聚合物基导体中的快速锂离子( Li )传输是绝望的需求,但仍然是一个严峻的挑战。在此,我们设计了一类基于含有短聚环氧乙烷( PEO )和聚二甲基硅氧烷( PDMS )侧链的混合接枝嵌段共聚物( mGBCPs )的固态电解质。PEO和PDMS的强不混溶性导致了有序相分离纳米结构的形成。在不同体积分数的PEO / PDMS嵌段中观察到了不同的形貌,包括双回旋体、六角开孔的片层、六角填充的和片层。通过改变PEO侧链长度,与自由PEO链共混,考察PEO的链迁移率对Li输运的影响。我们证明,将mGBCP与游离的无定形PEO链物理共混可显著促进Li的导电,制备了室温电导率可达2.0  × 10 - 4   S / cm的固态电解质。